| Applicable Heat Treatment | Normalization, annealing, quenching and tempering, Case Hardening, Nitriding, Carbon Nitriding, Induction Quenching |
| Applicable Finish Surface Treatment | Shot/sand blast, polishing, Surface passivation, Primer Painting , Powder coating, ED- Coating, Chromate Plating, zinc-plate, Dacromat coating, Finish Painting, |
| Lead Time | About 20-120days from the receipt date of deposit for casting stainless steel |
Chemical Elements
| C | Si | Mn | P | S | Cr | Mo | Ni | Cr+Mo+Ni |
| 0.42~0.50% | ≤0.4% | 0.5~0.8% | ≤0.045% | ≤0.045% | ≤0.4% | ≤0.1% | ≤0.4% | ≤0.63% |
The main manufacturing equipments
| Name&Description | Capacity | Quantity |
| 3600Thydraulic press | Max. single forging in 18T | 1 |
| 2000T hydraulic press | Max. single forging in 9T | 2 |
| 800 hydraulic press | Max. single forging in 5T | 1 |
| 6T electrical hydraulic hammer | Max.single forging in 5T | 1 |
| 3T electrical hydraulic hammer | Max.single forging in3T | 1 |
| Air hammer | Max.single forging from250kg to 1000kg | 7 |
| Forging operation machine | Max.single forging from20T-5T | 7 |
| Heat treatment Furance | Max.8000*5000*1500mm | 11 |
| CNC drilling machine | Max.5000mm | 2 |
| Vertical lathe | From 1600 to 5000mm | 60 |
| Horizontal lathe | Max.5000mm | 70 |
| Band sawing machine | 260-1300mm | 36 |